No second pic is after applying the sealer. I am wondering if it is because the hull is getting hotter from the heat, and when I am applying the sealer its drying quicker in some areas?
The first pic is before applying the sealer, nice and clear no blotchyness, second pic you can see the pad marks from the da. I finished with rupes on the blue hard foam pad.
Thx for the response. rupes compounds, flex rotary, finished with rupes hard foam on flex beast. Factory gel. Maybe its the humidity, or temp.? I am in so fla.
Da Pads leaving pad marks: Any thoughts on why after doing my correction on darker colored hulls, paint or gel.
When I apply the sealer with the da, I can see the pad marks. Sometimes it is barely noticeable sometimes it is quite noticeable.